Expert report review
Rebound hammer or cores: what does a reviewer check when the opposing expert says the concrete is too weak?
A rebound hammer measures surface hardness, and a drilled core measures compressive strength. ASTM C805/C805M-25 says the rebound test "is not suitable as the basis for acceptance or rejection of concrete", while ACI 318-19, where it permits cores, treats concrete as adequate if three cores average at least 85 percent of the specified strength. A reviewer starts by asking which of the two the opposing report actually relies on.

What does a rebound hammer measure, and what does a core measure?
The hammer gives a rebound number from a spring-driven steel mass striking the surface. A core is a cylinder of concrete drilled from the structure and crushed in a press to find the compressive strength of the in-place concrete.
ASTM C805/C805M-25, listed as active and last updated on June 19, 2025, opens with its scope: "This test method covers the determination of a rebound number of hardened concrete using a spring-driven steel hammer." The result is a number on the hammer's scale, not a strength. Section 5.1 describes the use: the method is applicable "to assess the in-place uniformity of concrete" and "to delineate variations in concrete quality throughout a structure."
ASTM C42/C42M-20, active since its update on May 5, 2020, covers "obtaining, preparing, and testing cores drilled from concrete". Under section 3.1 the cores serve "to determine the compressive, splitting tensile, and flexural strength of in-place concrete." Section 3.2 adds that specimens are generally obtained "when doubt exists about the in-place concrete quality".
So the two methods answer different questions. The hammer says where the concrete differs from the rest of the element. The core says how strong the concrete is at the place it was taken. An opposing report that converts rebound numbers into a strength value and compares that value with the specified strength has to explain how it bridged the gap.
Can a rebound hammer reading alone prove that the concrete fails the specification?
Not under its own standard. Section 5.5 of ASTM C805/C805M-25 says the method is not suitable as the basis for acceptance or rejection of concrete, and the technical literature reviewed here says the same.
The wording of section 5.5 is short: "This test method is not suitable as the basis for acceptance or rejection of concrete." A report that rejects a slab or a column on rebound numbers alone uses the test for a purpose its standard excludes. Under Rule 702(c) and (d) of the Federal Rules of Evidence that is a question about reliable methods and their reliable application.
The American Society of Concrete Contractors' technical checklist "Concrete Core Testing" (June 2008), written against ACI 318-08, quotes the ACI text on nondestructive tests, the impact hammer among them: they are "of value primarily for comparisons within the same job rather than as quantitative measures of strength."
A state-of-the-art review by Md Shah Nur Alam Sourav and Salam Al-Sabah of Arup and Ciaran McNally of University College Dublin reaches the same conclusion: the rebound test "should not be used for the basis of acceptance or rejection of concrete". It cites Malhotra's report of a deviation of plus or minus 15 to 20 percent in strength assessment for laboratory control specimens, a figure for specimens made and cured in a laboratory.
When can rebound numbers be converted into strength?
Only through a relationship established for the concrete in question. ASTM C805 section 5.4 requires a strength-rebound relationship for a given concrete, and limits the manufacturer's curves to indicating relative strength.
Section 5.4 of ASTM C805/C805M-25 states that "it is necessary to establish a relationship between strength and rebound number for a given concrete." The relationship supplied by the hammer's manufacturer may be used only to indicate relative strength. A report that reads strength values off the chart printed on the instrument has not done what section 5.4 asks.
Laboratory work shows why the relationship has to be specific. Baitollah Badarloo and Petr Lehner tested 150 cubes and reported in Infrastructures (vol. 8, art. 155, 2023) R-squared values "greater than 0.8" between hammer values and press strength. They also found that the manufacturer's chart "is lower than the experimental data", that the correlation equations differ by test direction, and that their results are limited to the concrete classes they tested and "cannot be applied to high-performance concrete".
For field work the Dublin review cites Szilágyi and Borosnyói, who suggested using the rebound hammer within the domain of each strength model, and Ireland's National Roads Authority, which advises using in-situ tests after calibrating their results, usually by coring. A paper in EPJ Web of Conferences (vol. 355, 2026) on non-destructive testing of different mixes records a finding from earlier studies that "the measurement error significantly impacted the estimate quality more than the model error did."
For the reviewer the questions follow: which correlation did the expert use, how many paired hammer and core results stand behind it, what range of strengths it covers, and whether the readings in dispute fall inside that range.
What affects a rebound reading?
Under ASTM C805 section 5.2, the moisture content of the test surface, the type of form or finish, the vertical distance from the bottom of a placement and the depth of carbonation, among other factors.
Section 5.2 lists the factors in one sentence. The rebound number "is affected by factors such as moisture content of the test surface", the type of form material or finishing used for the surface, the vertical distance from the bottom of a concrete placement and "the depth of carbonation". Each factor can move the reading without any change in the strength of the concrete beneath.
A reviewer reads the test record against that list. Was the surface wet, dry or recently cleaned? Were readings on a formed wall compared with readings on a troweled slab? Were readings near the top of a lift compared with readings near the bottom? Was carbonation depth measured, and where? A report that does not record these conditions leaves its numbers without the context the standard itself names.
Direction of impact matters as well. The Badarloo and Lehner study was built around testing "in different directions" and found that the correlation equations differ. A report that mixes horizontal readings on walls with downward readings on slabs, and converts both with one curve, gives the reviewer a specific point to raise.
What if the rebound readings and the cores point in different directions?
The cores carry the strength question, because ASTM C42 measures compressive strength and ASTM C805 only a rebound number. The hammer data still serve to locate weaker zones and to choose where further cores belong.
Section 5.1 of ASTM C805/C805M-25 gives the hammer its role: to assess in-place uniformity and to delineate variations in concrete quality throughout a structure. Section 3.2 of ASTM C42/C42M-20 gives cores theirs: they are taken when doubt exists about the in-place concrete quality. Read together, the hammer survey identifies the doubt and the cores resolve it.
A relationship under C805 section 5.4 is built from paired results, a rebound number and a core strength at the same location. If the opposing report presents both, the reviewer lists the pairs on a drawing and checks whether the weak rebound zones were cored at all, and whether the three cores per low strength test that ACI 318-19 section 26.12.6.1 calls for came from the zone in dispute or from elsewhere in the element.
How are cores judged under ACI 318?
Under section 26.12.6.1 of ACI 318-19, three cores are taken per strength test below the acceptance limit, once low strength is confirmed. They pass if they average 85 percent of the specified strength and none is below 75 percent.
The American Concrete Institute's FAQ on low-strength cylinder results, written for ACI 318-19, explains the sequence. If a strength test of standard-cured cylinders falls below the specified compressive strength by more than the limit allowed for acceptance, steps must be taken so that the structural adequacy of the structure is not jeopardized. Cores drilled under ASTM C42 are permitted if the likelihood of low-strength concrete is confirmed and calculations indicate that structural adequacy is significantly reduced. Then "three cores must be taken for each strength test that falls below the specified compressive strength by more than the limit allowed for acceptance."
The criteria are two: "the average of three cores is equal to at least 85 percent of the specified compressive strength" and "no single core is less than 75 percent of the specified compressive strength." The FAQ adds: "The building official should apply judgment as to the significance of low test results." It also states that "These requirements are applicable only for evaluation of in-place strength at the time of construction", and that strength evaluation of existing structures is covered by Chapter 27 of ACI 318-19.
ASTM C42 itself sets no pass or fail line. Note 4 says that the specifier of tests "should establish in the project specifications the acceptance criteria for core strengths" and gives the ACI 318 criteria only as an example. A reviewer therefore checks which criterion the opposing report applied, and whether the contract and specifications adopted it.
What can go wrong with core tests?
Location in the element, core orientation, moisture conditioning, the condition of the drilling equipment and the length to diameter ratio all change the measured strength. ASTM C42 names each of these in its significance and use section.
ASTM C42/C42M-20 section 3.3 states that "Concrete strength is affected by the location of the concrete in a structural element" and that "Core strength is also affected by core orientation relative to the horizontal plane". Section 3.4 adds moisture: core strength "is affected by the amount and distribution of moisture". Section 3.5 names "the condition of the coring apparatus, and the care used in removing cores", and section 3.7 the length to diameter ratio.
Section 3.5 also warns against direct comparison with cylinders. A core's compressive strength will generally be lower than that of a properly molded and cured cylinder tested at the same age, and "there is no unique relationship between the strengths of these two types of specimens".
The ASCC checklist turns these points into practical steps under ASTM C42-04: place each core in a sealed plastic bag or nonabsorbent container to prevent moisture loss, keep it sealed "for at least 5 days after last being wetted and before testing", aim for a length of "between 1.9 to 2.1 times the diameter", and apply the C42 correction factors for length to diameter ratios between 1 and 2. It also gives a minimum diameter of 3.70 in.
A reviewer asks for the coring log and the laboratory sheet. They show where each core came from, its orientation, the date drilled and tested, how it was stored, its dimensions and any correction applied. Gaps in that record are review points in their own right.
How did a court treat core evidence in a slab strength dispute?
In San Benito Supply v. KISAQ-RQ 8A 2 JV (N.D. Cal. 2015) a 6,000 psi slab never reached its strength. The court credited core and petrographic evidence of excess air and ruled against the ready-mix supplier.
The case arose on a Miller Act project at Fort Hunter Liggett. The ready-mix supplier sued for about $300,000 in unpaid invoices, and the concrete subcontractor counterclaimed for about $300,000 in replacement costs after the heavy-duty floor slab failed to reach its specified 6,000 psi. Magistrate Judge Howard R. Lloyd decided the case on January 28, 2015, after a nine-day bench trial, in a decision marked "not for citation".
The supplier's own expert drilled cores at seven slab locations and tested them at 101 days. The findings record that "Hichborn's core tests achieved an average compressive strength of only 4,210 psi, well less than what was needed." The memorandum refers to an adjusted average of 5,050 psi and concludes that "The heavy duty slab on grade was never going to get to 6000 psi."
A petrographer examined cores taken by the subcontractor's laboratory and found 6 to 7.4 percent air against a 4 percent design maximum, which he said reduced strength by 10 to 15 percent. The court credited that testimony, found that the mix design was not properly qualified and that the supplier added entrained air without authority, and awarded the subcontractor $55,035.13. The supplier took nothing.
In that case the core strengths answered how weak the slab was, and the petrographic examination of the same cores answered why.
What does the reviewer request from the other side?
The raw rebound readings with locations and conditions, the hammer's calibration record, the correlation data, the coring logs, the laboratory reports and any petrographic work. Rule 26(a)(2)(B) requires disclosure of the facts or data considered.
Rule 26(a)(2)(B) of the Federal Rules of Civil Procedure requires a retained expert's report to contain all opinions with their basis and reasons, "the facts or data considered by the witness in forming them" and "any exhibits that will be used to summarize or support them". For a concrete strength report those facts are each individual reading as well as the averages, the test grid on a drawing, the surface condition and carbonation measurements, the correlation used, and for cores the drilling log and laboratory sheets.
Where the reviewer needs new data, Rule 34(a)(2) lets a party request entry onto property the other side possesses or controls "so that the requesting party may inspect, measure, survey, photograph, test, or sample the property". A request to take additional cores names the locations and the method, and the written response is due within 30 days after service.
The checklist of points to raise follows from the standards above: rebound numbers used for acceptance contrary to C805 section 5.5; strength read from a manufacturer's curve contrary to section 5.4; conditions under section 5.2 not recorded; cores not conditioned or corrected under C42; and an acceptance criterion that the contract never adopted.
How does the review reach the court?
As a rebuttal report, deposition questions and the basis for a Rule 702 motion. A rebuttal on the same subject is due within 30 days after the other side's disclosure unless the court orders otherwise.
Under Rule 26(a)(2)(D)(ii), evidence "intended solely to contradict or rebut evidence on the same subject matter" identified by another party is disclosed "within 30 days after the other party's disclosure", absent a stipulation or court order. A rebuttal report on concrete strength answers the opposing tests point by point and, where the data allow, states what the cores or a proper correlation would show instead.
Rule 702 requires the proponent to persuade the court that it is more likely than not that the opinion rests on sufficient facts or data, comes from reliable principles and methods and applies them reliably to the facts. A strength opinion built on a test its own standard calls unsuitable for acceptance, or on a curve the standard limits to relative strength, is the kind of opinion a reviewer flags under that rule.
What does IAE do when the other side's report says the concrete is too weak?
IAE prepares reviews of the opposing construction expert's report and rebuttal reports for US cases, with deposition questions, each point tied to a rule or standard, in up to 5 business days after format and cost are confirmed.
The IAE page on reviews of construction expert reports is written for attorneys facing the other side's construction expert on a leak, defective work or a repair estimate. The reviewer reads the opposing report with its exhibits and the data the expert considered, tests each opinion against the data behind it and ties each point to a rule or a standard.
The client sends the opposing report with its exhibits, the rebound and core data disclosed, the laboratory reports, the specifications for the concrete and the deadlines, and describes what to check. The secretariat confirms receipt the same day. Within one business day IAE confirms the format, the cost, the deadline and the specialist from its registry, and the client approves the candidate and the CV before work starts. The document is issued in up to 5 business days after the format and cost are confirmed, and cases with tight deadlines have a 48-hour rush.
Every specialist is a member of the public IAE registry and can be verified by Member ID or QR code. The specialist confirms in the document that he or she has no interest in the outcome of the case. IAE is not a law firm and does not advise on case strategy. A review is evidence that the court weighs with the other materials, and neither IAE nor the reviewer guarantees the outcome.
Sources
- ASTM C805/C805M-25, Standard Test Method for Rebound Number of Hardened Concrete (ASTM)
- ASTM C42/C42M-20, Standard Test Method for Obtaining and Testing Drilled Cores and Sawed Beams of Concrete (ASTM)
- American Concrete Institute, FAQ: Low-strength cylinder test results (ACI 318-19)
- American Society of Concrete Contractors, Technical Checklist: Concrete Core Testing (June 2008)
- Sourav, Al-Sabah, McNally, Strength assessment of in-situ concrete for the evaluation of structural capacity: State of the art (UCD Research Repository)
- Badarloo, Lehner, Practical Aspects of Correlation Analysis of Compressive Strength from Destructive and Non-Destructive Methods in Different Directions, Infrastructures 8(11):155 (2023)
- Chandrashekar et al., Effect of Concrete Mix Design on Non-Destructive Test Results for Strength Evaluation, EPJ Web of Conferences 355, 02003 (2026)
- United States ex rel. San Benito Supply v. KISAQ-RQ 8A 2 JV, No. C13-00469 HRL (N.D. Cal. Jan. 28, 2015) (Justia)
- Federal Rules of Civil Procedure, Rule 26 (LII, Cornell Law School)
- Federal Rules of Civil Procedure, Rule 34 (LII, Cornell Law School)
- Federal Rules of Evidence, Rule 702 (LII, Cornell Law School)
Read also
All articles
Is the opposing construction expert qualified for every opinion in the report, and how is the qualification challenged?
Rule 702 admits a construction expert qualified "by knowledge, skill, experience, training, or education", and courts test that qualification opinion
Sinkhole claim denied in Florida: how does a reviewer test the insurer's engineering report?
When a Florida insurer denies a sinkhole claim after testing, the denial rests on the report of the engineer or geologist it hired. Sections 627.706
Cast iron pipe claim: what does a reviewer check in the opposing plumbing or engineering expert's report?
In a cast iron pipe dispute the expert's words about cause and duration decide coverage. In State Farm Florida Insurance Co. v. Feltes (Fla. 6th DCAExpert report review
Ready to discuss your case?
Send the materials: the secretariat will confirm the format, cost, deadline and the specialist within one business day.